  1. Article: Marginal adaptation of Spinell InCeram and feldspathic porcelain laminate veneers.

    Ghaffari, Tahereh / Hamedi-Rad, Fahimeh / Fakhrzadeh, Vahid

    Dental research journal

    2015  Volume 13, Issue 3, Page(s) 239–244

    Abstract: ... for the construction of DuCeram and InCeram laminate veneers. An image-analysis program was used to measure the gap ... Background: This in vitro study investigated the marginal fit of two porcelain laminate veneers ... for InCeram and DuCeram were, respectively, 114.4 ± 40.81 and 282.3 ± 82.82. Independent t-test revealed ...

    Abstract Background: This in vitro study investigated the marginal fit of two porcelain laminate veneers to help the selection of more accurate veneers in discolored teeth.
    Materials and methods: Thirty impressions of metal master die created from the prepared labial surface of an acrylic maxillary central incisor were made and poured with Type IV stone. The dies were distributed into test groups (n = 15) for the construction of DuCeram and InCeram laminate veneers. An image-analysis program was used to measure the gap between the veneers and the master die at the labial, lingual, and proximal margins. Statistical analysis was performed with repeated measures ANOVA. Independent t-test was used to compare the mean values between the two groups. Values of P < 0.05 were judged to be significant.
    Results: Differences between marginal fit of two groups were significant (P < 0.001). The overall mean marginal gap values (μm) for InCeram and DuCeram were, respectively, 114.4 ± 40.81 and 282.3 ± 82.82. Independent t-test revealed significant differences between the marginal gaps of two materials at different predetermined points.
    Conclusion: Within the limitations of this study, the marginal gap in InCeram laminate veneer was within the clinically acceptable standard set at 120 μm.
    Language English
    Publishing date 2015-11-07
    Publishing country Iran
    Document type Journal Article
    ZDB-ID 2418290-4
    ISSN 2008-0255 ; 1735-3327
    ISSN (online) 2008-0255
    ISSN 1735-3327
    DOI 10.4103/1735-3327.182183
    Database MEDical Literature Analysis and Retrieval System OnLINE

    More links

    Kategorien

  2. Article ; Online: Marginal adaptation of Spinell InCeram and feldspathic porcelain laminate veneers

    Tahereh Ghaffari / Fahimeh Hamedi-Rad / Vahid Fakhrzadeh

    Dental Research Journal, Vol 13, Iss 3, Pp 239-

    2016  Volume 244

    Abstract: ... for the construction of DuCeram and InCeram laminate veneers. An image-analysis program was used to measure the gap ... Background: This in vitro study investigated the marginal fit of two porcelain laminate veneers ... for InCeram and DuCeram were, respectively, 114.4 ± 40.81 and 282.3 ± 82.82. Independent t-test revealed ...

    Abstract Background: This in vitro study investigated the marginal fit of two porcelain laminate veneers to help the selection of more accurate veneers in discolored teeth. Materials and Methods: Thirty impressions of metal master die created from the prepared labial surface of an acrylic maxillary central incisor were made and poured with Type IV stone. The dies were distributed into test groups (n = 15) for the construction of DuCeram and InCeram laminate veneers. An image-analysis program was used to measure the gap between the veneers and the master die at the labial, lingual, and proximal margins. Statistical analysis was performed with repeated measures ANOVA. Independent t-test was used to compare the mean values between the two groups. Values of P < 0.05 were judged to be significant. Results: Differences between marginal fit of two groups were significant (P < 0.001). The overall mean marginal gap values (μm) for InCeram and DuCeram were, respectively, 114.4 ± 40.81 and 282.3 ± 82.82. Independent t-test revealed significant differences between the marginal gaps of two materials at different predetermined points. Conclusion: Within the limitations of this study, the marginal gap in InCeram laminate veneer was within the clinically acceptable standard set at 120 μm.
    Keywords Dental marginal adaptation ; dental porcelain ; dental veneer ; Medicine ; R ; Dentistry ; RK1-715
    Subject code 670
    Publishing date 2016-01-01T00:00:00Z
    Publisher Isfahan University of Medical Sciences
    Document type Article ; Online
    Database BASE - Bielefeld Academic Search Engine (life sciences selection)

    More links

    Kategorien

To top